What 800 V Architectures Change for Die Cast EV Housings

An RFQ reached us in March with 800 V in the title block and one instruction underneath it: increase wall thickness for the higher voltage. No number, no target. We quoted the part in the same 1.5–2.5 mm band we use for a 400 V motor controller housing, because the wall was never the voltage question.

What the voltage changes sits around the metal, not in it: the distance from a live conductor to the grounded shell, the length of the path across its surface, the voids and edges where partial discharge starts, the heat that has to leave through it, and the seams that must stay dry. Those five land on different features, and only one is wall thickness.

800 V does not call for a thicker wall

The wall stays where it was; the distance between live metal and grounded metal is what has to grow.

Double the bus voltage and the field across an unchanged gap roughly doubles, so the design adds distance or adds insulation. At the same power it also halves the current, so conductor loss falls while switching loss and power density climb, and the heat moves into the inverter and out through the housing. The shell is grounded, which makes distance its only contribution: insulation on the conductor side belongs to the busbar and module supplier, and that division decides who owns a failed withstand test.

The rule that governs the gap is insulation coordination, and IEC 60664-1:2020 covers equipment up to 1 000 V AC and 1 500 V DC, so an 800 V DC bus sits inside its scope. It derives clearance from the expected overvoltage and creepage from pollution degree and the material’s tracking behaviour, which is why a drawing that says only “800 V” tells a caster almost nothing.

Boundary condition400 V class800 V classWhat it moves in the casting
Air clearanceSized from bus voltage and overvoltage categoryRoughly double the gap for the same coordinationTerminal window, phase barriers, feedthrough spacing
Creepage pathA surface path over a dirty, damp mouldingLonger, and far more sensitive to surface qualityAs-cast skin in the HV cavity, rib roots, machined lands
Partial dischargeTolerated in most designsManaged, because voids and edges become the failure siteSkin porosity, edge radii, blast media, cleanliness
Heat fluxLoss spread over a larger, cooler packageSame power at half the current, higher power densityPad flatness, wall in the heat path, jacket
SealingCoolant and wash water kept out of a low-voltage cavitySame, plus moisture and conductive debris in the HV cavityGasket groove, insert interfaces, cleanliness class

I once quoted a housing with a 4 mm wall everywhere “for 800 V” while the shortest air gap in the assembly was 14 mm. The extra metal added mass and cycle time and changed nothing electrical; the unspecified terminal window tolerance put the first batch into rework.

The five jobs the housing has to do

At 800 V the casting has to hold a gap, keep a surface path long, suppress discharge at voids and edges, carry heat out of a denser inverter, and keep the cavity dry — five jobs that pull on each other.

The first two are settled in the tool. The third is process: a vacuum-assisted fill at 50–200 mbar removes gas that would otherwise sit in the skin, and does nothing for shrinkage, which is a feeding problem in the same wall. The fourth is a machining promise: 0.3–0.5 mm flatness on the pad face, depending on size. The fifth is joint design: a gasket groove cut in the same setup as the bore stays coaxial.

JobHow the casting does itWhat we can show at PPAP
Hold the air gapCast phase barriers, controlled terminal window, no draft thinningReport per ISO 1101, capability on controlling dimensions
Keep creepage longSmooth skin in the HV cavity, radiused rib roots, machined landSurface acceptance standard, profile on the path, radiograph
Suppress dischargeVacuum-assisted fill, no cold shuts on a barrier, radiused edgesASTM E505 sampling, first-article CT, edge condition
Bond to groundMasked conductive pad, no coating under the strapContact resistance after coating, ISO 2360 with the pad masked
Carry heat outFlat pad face, wall maintained through the heat pathFlatness 0.3–0.5 mm, wall section from the CT, jacket leak test
Keep the cavity dryGasket groove cut with the bore, sealed insert interfacesPressure decay 0.3–1.0 bar or helium, VDA 19.1 report
Aluminium 800 V inverter housing on a die casting cell, cast phase barriers and terminal window visible

Where a die casting is weakest at 800 V

Three failure modes separate an 800 V housing from a 400 V one that looks identical on the drawing, and all three come from the process rather than the voltage.

Porosity that only appears after the boring bar

A pore that sat harmlessly inside a 400 V wall becomes a leak path or a field concentration once machining opens it. The bad ones are sub-surface: gas porosity from a cold fill, shrinkage where a section could not be fed, cold shuts on a barrier face. Vacuum takes out the first; the second needs a changed section or gate. A radiograph taken before machining will not show a pore that only reaches the surface once the cutter has been through.

So we plan the cut and the inspection together. If the seal land and cavity walls are opened by machining, the radiograph sample sits after the cut, and the leak test runs on the finished part. Impregnation seals a leak path; it does not restore a creepage wall that has been hollowed out, and the resin changes how the surface behaves under discharge.

The insert interface is a gap with a voltage across it

Every 800 V housing has something cast in or pressed in: a busbar feedthrough, a threaded boss, a grounding stud. Aluminium moves about twice as far as steel over the same temperature rise, so the interface breathes on every thermal cycle. A 0.1 mm step there is a coolant seep at 400 V and a tracking path at 800 V.

Keep inserts out of the gasket groove’s clamping band, put a machined counterbore behind a feedthrough so the seal sits on cut metal rather than cast skin, and specify insert material and plating on the drawing. A steel insert with wash water in the cavity is also a galvanic couple, and the corrosion product is conductive.

One surface, two jobs: insulate and conduct

The same outer skin has to resist tracking along a creepage path and carry a low-impedance bond at the ground strap, and the coating schedule is where projects lose it. Powder coat and e-coat build a dielectric layer exactly where the strap lands; masking the pad fixes the bond but leaves a bare edge that corrodes under salt spray per ISO 9227. Anodising on a high-silicon die casting is decorative, not an insulating barrier.

We write the coating map on the drawing: which faces are coated, which are masked, which are machined after coating. Blasting leaves media in a pocket with no drain, and a bead in a cavity is a void with a field concentration at its edge. EMI shielding and the ground path are one conversation: a seam that is not bonded is an antenna, and a strap on coating is a resistor. A housing that is not properly grounded shows up as a failed bond check.

Running 400 V and 800 V housings on the same line

Yes, and most of our programmes do, because the process does not fork at the voltage: the same 350–3050T cell, ADC12 or AlSi10MnMg, vacuum system and 150+ four- and five-axis machines. What forks is tooling content, fixtures and end-of-line test.

In the tool, the 800 V variant usually needs a different core package for the phase barriers and terminal window, sometimes a different gate position because the window moved. That is an insert, not a new tool. The line-level change that gets underestimated is the test station: a withstand test and a partial discharge measurement need an enclosure, an interlock and a safety case, and they run on the assembly rather than the bare casting. Mixing the two parts also means error-proofing — different part numbers, different fixtures, a scan check before test.

How the inspection list grows

The casting tests barely change; the assembly tests do, and the caster’s job is to keep geometry and surface out of the failure report.

Air leak stays first. We test the coolant jacket and the HV cavity separately at 0.3–1.0 bar pressure decay, or with helium where the limit is tighter, and the specification has to come from the customer because a casting has no intrinsic leak rate. Then cleanliness: VDA 19.1, mg per part plus particle size, because a conductive chip in the wrong place bridges a path that was dimensioned correctly.

Withstand voltage, insulation resistance and partial discharge belong to the assembly, and that is not a dodge. Partial discharge is measured as apparent charge under IEC 60270:2025, and it depends on conductor insulation, busbar geometry, the air in the cavity and the casting surface at once. A bare shell has nothing to discharge from. What we can do is guarantee the inputs: the gap, the surface, a void-free barrier, and a leak and cleanliness record that survives an audit.

Pressure decay leak test rig with an aluminium EV housing clamped on a sealing plate
CheckMethod or standardWhat it catchesWhere it runs
Leak, pressure decay0.3–1.0 bar, limit set by the customerA path through a wall, a seal land or an insert100% inline, after machining
Leak, heliumTracer gas where the limit is tighterPinholes and connected porosity a decay test missesSampling or 100%, after machining
CleanlinessVDA 19.1, mg per part plus particle sizeConductive debris bridging a creepage pathAfter the wash, per lot
CoatingISO 2360, ISO 2409, ISO 9227Coating under a ground strap, a bare edge that corrodesCoated parts, per lot
RadiographyASTM E505Porosity in a barrier, a seal land or a thin ligamentFirst article plus sampling
DimensionalCMM, ISO 1101; flatness 0.3–0.5 mmWindow position, barrier height, pad flatnessFirst article plus audit

When die casting is the wrong answer

It is the wrong answer whenever the part is asked to be the insulation, or the volume cannot pay for the tool, and those two cover more 800 V projects than the voltage does.

Aluminium conducts. A housing cannot be the dielectric barrier between a live busbar and the outside world; it can only be the grounded shape that sets distance and surface. If the wall itself must insulate, that is a polymer housing or a lined part, and no casting process changes the physics. Where a pressure boundary has to be leak-free through a section too thin to feed, a 1.2 mm ligament over a long channel is possible, but it is a porosity argument, not a drawing note.

Volume decides the rest. Below roughly 10 000 parts a year, tooling amortisation usually pushes the part to sand or gravity, where A356 at 5–8 % elongation is easier to feed and weld. Above that, a 350–3050T cell with vacuum assist is cheaper per part and holds the 1.5–2.5 mm band. Large flat covers that must stay flat after T6 are a third case, and the answer is sometimes a casting, a stamping and a gasket rather than one part that distorts.

FAQ

Does an 800 V housing need a thicker wall than a 400 V one?

No. The wall stays in the 1.5–2.5 mm band at both voltages, with local 1.2 mm sections over short runs. What changes is the air gap and the creepage path, which are geometry, plus surface quality and cleanliness inside the HV cavity.

Can a die caster partial-discharge test a bare housing?

Not in any useful sense. Partial discharge is a property of the assembly, measured as apparent charge per IEC 60270, and it depends on the insulation system, busbar geometry and the air in the cavity as much as on the casting. The caster supplies the gap, the surface, the void-free barrier and the cleanliness record.

Is impregnation acceptable on an 800 V housing?

It seals a leak path and it is used on production parts, but it is a process fix rather than a design fix. It does not restore a creepage wall that machining has opened, and it does not remove a void on a barrier face.

Can 400 V and 800 V housings run on one production line?

Yes, on the same cells and alloy, and most programmes do. The differences are the core package and terminal window in the tool, separate fixtures, an end-of-line test with enclosure and interlock, and error-proofing so a 400 V part cannot reach an 800 V test station.

So the useful question is not how thick the wall should be. It is which surfaces carry the field, how long the path across them is, which voids sit on those surfaces after machining, and what the drawing says about all three. A drawing that answers those four is quotable; one that says 800 V and a wall thickness gets argued about at the first leak test.