A drawing arrived last quarter with three requirements in the title block: 800 V platform, 3.0 mm nominal wall, leak-tight. Nine pages of geometry followed. None of them said which wall was a pressure boundary, what “leak-tight” meant in mbar per minute, or how round the stator bore had to be after machining. Those three omissions decide the tool, the process and the price. The voltage class barely enters the quotation.
That gap is normal. A drive motor housing is where an EV programme’s electrical, thermal and NVH targets land at once, and the drawing is usually written by someone who owns only one of them. What follows is what I would ask before quoting a 2026 drive motor housing, in the order the answers change the process.

800 V changes clearance, not nominal wall thickness
At 800 V the nominal wall stays in the same 1.5–2.5 mm band as at 400 V; what changes is where metal may sit relative to the live conductors. Double the bus voltage and you roughly double the dielectric stress across an unchanged gap, so the design needs more distance or better insulation. The housing is grounded, which means distance is its only contribution.
That distance shows up as geometry, not thickness: a wider terminal window, phase barriers cast into the end wall, no thin fins crossing a creepage path, and a smoother as-cast surface in the HV cavity, where a cold shut gives moisture somewhere to sit. Thickening appears at feedthrough bosses where a thread needs depth, at seal grooves and over a cooling channel, but none of that is a voltage decision.
I have quoted a housing with a 4 mm wall everywhere “for 800 V” where the shortest air gap in the assembly was 14 mm. The wall added mass and changed nothing electrical. The terminal window tolerance, which nobody had specified, put the first batch into rework.
| Decision | 400 V class | 800 V class | What it does to the casting |
|---|---|---|---|
| Bus voltage | About 400 V nominal | About 800 V nominal | Sets the gap the grounded housing must guarantee, not its wall |
| Governing rule | Clearance and creepage in the HV safety case | Same rule, roughly double the distance | Terminal window and phase barriers grow; nominal wall does not |
| Where thickness moves | Thread bosses, seal grooves | Those, plus HV feedthrough bosses | Local bosses and ribs, not a global wall increase |
| Thermal load | Resistive loss dominates | Lower current for the same power, higher power density | The cooling jacket stays; its geometry matters more than the alloy |
A cast-in cooling jacket turns one wall into two
An integrated cooling channel makes the inner wall a pressure boundary, and that ligament decides whether the part leaks into the motor cavity. The outer wall handles stiffness and little else. The ligament between channel and bore carries coolant pressure plus the boring allowance, and if it comes out at 1.5 mm while the core has shifted 0.4 mm, the channel breaks through and the part is scrap, not rework.
Channels are formed with soluble cores, or the jacket is cast separately and welded on. Cores add cycle time and a wash-out step; welding adds a joint to leak-test and a distortion step after it. HPDC can cast the channel, but the wall around it is designed for core stability first and heat transfer second.
The thermal case for a thin wall is stronger than the alloy case. In AlSi10MnMg, conductivity at 50 °C sits between 125 and 138 W/(m·K) depending on cooling rate, slower cooling giving the higher number (Materials, 2024). Run the arithmetic per unit area: 125 through 2.5 mm is about 50,000 W/(m²·K), 138 through 3.5 mm about 39,400. The thinner wall wins by a quarter even though its metal conducts worse, so the wall stays thin where heat leaves and thick only where pressure or a thread demands it.

Roundness and seal-face flatness are machining promises
The stator bore is round because of how the part was held and cut, not because it was cast well. A near-net bore from the die is an allowance; the boring bar makes the circle. What goes wrong between the two is residual stress and clamping: a three-jaw chuck closes a 200 mm bore into a triangle, and the CMM then reports the fixture, not the part.
Two habits remove most of that argument. Machine the bore, the seal face and the mounting face in one setup from one datum, which is what our 150+ four- and five-axis cells are arranged to do, holding ±0.05 mm on machined features. Then measure at a stated temperature: a 200 mm aluminium bore grows about 0.046 mm per 10 °C, the same order as the roundness being argued about.
Seal-face flatness is the other half. We hold 0.3–0.5 mm depending on face size, and anything above roughly 400 mm across needs its own conversation about clamping and support: routine on a 120 mm cover face, a fixture design on a 420 mm front cover. Cut the groove in the same setup as the bore so the two stay coaxial, and test the leak after that cut. Roundness also sets the air gap: on a typical 0.5–1.0 mm gap, 0.05 mm of ovality is 5–10 % of it.
Thin wall or structural: choose the failure mode first
1.5–2.5 mm is the working band for a housing wall; 1.2 mm is possible over short sections, and below that the alloy freezes before the cavity fills. Thin walls buy mass, conductance and less metal to shrink. They cost fill time — 20–60 ms leaves no time to bleed heat — porosity in the bore wall that appears only after the boring bar opens it, and stiffness: a 1.5 mm wall springs under clamping, so the cut that was on size in the fixture is out of size on the CMM. Solvable, but priced.
Structural duty pulls the other way. If the housing is in the load path the requirement is elongation, and elongation is an alloy decision: ADC12 sits at 1–3 %, AlSi10MnMg at 8–12 %. A part that is structural and thin-walled everywhere at 2 mm does not exist; the design has to name which 20 % carries the load and let the rest be stiff. The limits of 1.2 mm thin-wall casting are worth reading before that call.
Vacuum HPDC plus T6: what the pair actually delivers
Vacuum removes the gas that would otherwise expand in the solution furnace; T6 buys strength and ductility and charges for it in distortion and a changed failure mode. Vacuum at 50–200 mbar addresses gas porosity, which is why porosity reduction from vacuum gets measured rather than assumed. It does nothing for shrinkage porosity, a feeding problem that is still there after heat treatment.
The T6 sequence — solution treatment near 500 °C, quench, age — does two things to a die casting. Gas pores expand during solution treatment and blister on any surface machined afterwards. And it changes the phases: in high-vacuum die-cast AlSiMgMn, T6 alters the hardness and Young’s modulus of individual phases and changes the crack path, so the as-cast and T6 versions of the same part fail differently (Materials, 2019).
That is why I ask for the heat-treat state per zone, not per part. A bearing seat wants T6 for strength. A 400 mm cover face wants T5 or as-cast, because the quench will move it and moving it costs more than the strength is worth. Specifying T6 globally is how a project ends up straightening parts.
| Item | Vacuum HPDC | Gravity die casting | Consequence for a housing |
|---|---|---|---|
| Practical minimum wall | 1.2–1.5 mm on short sections; 1.5–2.5 mm general | 3–4 mm | Only HPDC gets close to the mass target |
| Fill time | 20–60 ms | Seconds | HPDC needs vacuum and a designed gate; gravity tolerates a poorer one |
| Dominant porosity | Gas, controlled by vacuum level | Shrinkage, controlled by feeders | A leak found in service traces back to a different cause |
| T6 response | Blister risk if gas pores remain | Routine | HPDC plus T6 needs the vacuum proven, not promised |
| Dimensional consistency | Die-limited, high | Mould and core variability | HPDC is the only route to 100 % leak testing economically |
| Tooling and volume | High tool cost, high volume | Lower tool cost, low volume | Below about 10,000 parts a year, gravity is worth pricing |
Test the leak after machining, and write the spec before the tool
A leak test on a raw casting proves little if the boring bar opens the leak path two operations later. Boring, milling the seal groove and drilling the mounting holes all expose subsurface pores, and those are the paths that fail at the customer.
So the sequence is: machine, clean, test. We run 100 % in-line pressure-decay testing at 0.3–1.0 bar against the customer’s limit, with helium for tighter limits; the limit itself comes from the customer as a written specification. Without medium, pressure, dwell, reject value, temperature and masked cavities written down, two labs can test the same part and disagree, and the argument lands on the supplier.
Machining strategy decides how much of that risk you carry. One setup for bore, seal face and mounting face keeps the coaxiality stack short. Coolant-through tools and a defined deburr keep chips out of the cooling channel, and cleanliness gets verified to VDA 19.1 with a milligram-per-part number rather than a visual check — the discipline behind guaranteeing airtightness in EV die-cast housings.
For internal soundness, radiography is a sampling tool, not a guarantee. ASTM E505 gives the reference images and acceptance levels, and a 2024 comparison of low-cost radiography, industrial radiography and micro-CT found single-projection images noisy enough to miss pore classes; the ground truth sat with CT (Materials, 2024). Use CT on the first article and radiograph at a stated rate.
| Field | Why it changes the verdict |
|---|---|
| Test medium | Air decay and helium find different leak sizes; helium reaches tighter limits |
| Pressure and direction | Internal pressure, external submersion and vacuum decay load the seal differently |
| Dwell and stabilisation | Short dwell reads the fixture’s thermal drift as a leak |
| Reject value and units | mbar·L/s, sccm and “no bubbles” are not interchangeable |
| Masked features | Open ports and machined-through holes must be sealed or the test is meaningless |
What to ask a supplier in 2026
Ask for evidence you can audit without a site visit. The answers separate a caster who has run this part family from one who has run something similar.
- Which machine, and the projection area calculation. Tonnage follows projected area, not part weight; we quote 350T to 3050T across 13 cells.
- Vacuum level logged per shot. A catalogue figure is not a process record; ask for the trace from a production run.
- The leak specification with numbers. If the supplier cannot restate your six fields, they are testing to habit.
- A CMM report with the datum scheme, plus Cpk on functional dimensions: 1.33 is our floor, 1.67 on safety features.
- Heat treatment in-house or subcontracted, with quench delay and distortion data. T6 is where a good casting becomes a bad machined part.
- Radiography and CT sampling plan with acceptance levels: E505 class, rate, and who reviews the films.
- PPAP Level 3 element list with an owner for each. IATF 16949:2016 and a VDA 6.3 grade A audit cover the system; PPAP covers your part.
- What they will not do. A supplier who names the wall, alloy or volume they decline is easier to trust on the rest. Our EV and automotive die casting work is quoted the same way.
Where this leaves a 2026 housing RFQ
The housing has stopped being a machined box. EV drive motor housing die casting is now a tolerance-and-leak job with a thermal problem, and the drawings that survive production specify zones, tests and evidence instead of global numbers. A 3.0 mm wall and the word “leak-tight” tell a supplier almost nothing.
Frequently Asked Questions
Does an 800 V drive unit need a thicker cast housing?
Normally no. The nominal wall stays in the 1.5–2.5 mm band. The voltage class changes clearance and creepage geometry — terminal windows, phase barriers, feedthrough bosses — which are local features. A global wall increase adds mass without improving insulation.
Can a die-cast housing hold stator bore roundness without a second boring operation?
Not to the numbers that matter for NVH. The die delivers an allowance; the finish bore comes from machining, and the result depends on clamping, residual stress and a single-setup datum. A casting round in the die can be oval after a three-jaw chuck.
Is vacuum HPDC enough for a cooling jacket that must hold pressure?
It is enough for the porosity, provided the ligament between channel and bore is designed for core shift and the part is leak-tested after machining. Vacuum does not fix a 1.5 mm ligament or a core that moves.
Should the leak test happen before or after machining?
After. Machining opens subsurface pores and creates the sealing surfaces, so a raw-casting test misses the failures that matter. Test the finished part to a written specification and keep the raw check as a process monitor.