In a machined automotive die casting, the biggest line in the quote is rarely the casting rate. It is the metal bought to make the blank heavier than the part, plus the machining hours spent removing it. Die casting value engineering therefore pays better than price negotiation: an as-cast face, a thinner section and one loosened tolerance the function never needed can take out more than a 10% cut in the press rate, and they keep taking it out on every part. How a die casting price is actually built shows which lines the supplier controls and which the drawing controls.

Where the cost actually sits in a die casting quote
Four lines carry most of a machined housing: metal, machining, casting conversion and scrap. The casting rate is one of them, and on a part machined on several faces it is rarely the largest.
A quote is built from blank weight, machining operations, press hours and tooling amortization, then multiplied by a yield assumption. Ask for those five numbers separately. A supplier who cannot split them is quoting from a catalogue; a buyer who cannot read them negotiates the only line that was already small.
| Cost line | What it covers | Illustrative share | What moves it | Who controls it |
|---|---|---|---|---|
| Aluminium, net of returns | Blank weight minus scrap credit on runners and biscuit | 40–55% | Part weight, wall and rib design, gate mass, alloy | Drawing, then die layout |
| Machining | Machine hours, fixtures, tools, deburr | 15–30% | Faces, setups, tolerance class, tool access | Drawing, then process plan |
| Casting conversion | Press time, energy, labour, die maintenance | 10–18% | Shot weight, cycle, cavity count, downtime | Process and volume |
| Tooling amortization | Die, trim tool, fixtures and gauges divided by volume | 5–15% | Tool complexity, slide count, annual volume | Drawing and volume |
| Scrap and rework | Casting scrap, leak rejects, machining fallout | 3–10% | Wall, draft, porosity, tolerance | Drawing and process window |
| Finishing and freight | Coating, packing, container | 3–8% | Surface spec, packaging, route | Customer spec |
The shares are illustrative, a spread across machined housings at 20,000–100,000 pieces a year rather than a benchmark. Put your own five numbers in their place; the order is what tells you where to spend engineering time.
Metal is the line most often misread. The blank is what the foundry buys, while runners and overflows return as scrap credit at a discount to the purchase price, so a heavy gate system costs real money even though it “returns”. Shipped weight divided by bought metal is a ratio you can compute from the drawing before any quote arrives.
Why the press rate is a weak lever
Press time runs in tens of seconds and is shared across everything in the shot, while metal is bought by the kilogram on every part. Ten percent off the casting rate trims a line that may be a sixth of piece price. Three hundred grams out of the blank trims the metal bill at every volume, and nobody renegotiates it next year.
Machining behaves the same way. A face that does not need cutting still costs a fixture, a program segment, a queue slot and an inspection record, and none of that disappears when the hourly rate drops. It is why two automotive die casting quotes usually differ by drawing more than by rate.
Rate negotiation still has a place: metal index, payment terms, volume tier, freight. It is worth doing and it is reversible, because the next RFQ takes it back. A drawing change is not, since the die carries it for the life of the programme.
The three features that move more money than the price
Blank weight, machined surface count and tolerance class, in that order. Draft and slide count follow, because they move tooling and scrap rather than the unit cost of a good part.
| Feature | As drawn | After review | Where the saving comes from | What it costs |
|---|---|---|---|---|
| Cosmetic cover face | Machined, 1.5 mm allowance, ±0.1 mm | As cast to ISO 8062-3 DCTG | One operation, one fixture, 1.5 mm of metal across the face | Cast surface finish; visible faces may need blasting |
| Boss for an M6 thread | 18 mm tall, cast pilot drilled and tapped | 10 mm boss with a thread insert | About 120 g of metal, shorter solidification | Insert cost and an assembly step; pull-out strength to validate |
| Machined faces | Three faces, three setups | Two faces, one setup | One fixture, one queue slot, one less positional stack | Fixture design and a 5-axis programme |
| Wall and rib section | 3.2 mm uniform wall | 2.4 mm wall, 1.5 mm ribs | 0.6 kg per part and a shorter cycle | Fill and die thermal balance; vacuum at the thin end |
| Draft on a deep wall | 0.5° over 90 mm | 1.5° over 90 mm | Fewer pulled walls, less polish time | 1.6 mm more stock at the parting line |
| Non-functional pad | ±0.05 mm, CMM on every part | ±0.25 mm, sample check | Inspection time and a rework loop | Nothing, if no part mates with it |
Blank weight comes first because it is paid twice, as metal and again as the machining that removes it. Dropping a housing that holds no pressure from a 3.2 mm wall to 2.4 mm with 1.5 mm ribs takes 0.6 kg off a 3 kg part, shortens solidification and leaves less shrink porosity to chase with vacuum. The floor is real: 1.5–2.5 mm is the band we quote, and 1.2 mm works over a limited length with vacuum and die thermal balance behind it.
Machined surface count is second because each extra setup adds a fixture, a positional tolerance and a queue. Single-setup work on a 4- or 5-axis cell removes the stack between operations, and the argument about which face is datum. Count the faces machined “for flatness” with nothing mating against them.
Tolerance class is third, and the one buyers defend hardest. We hold ±0.05 mm on machined features, key bores tighter, and going further costs cycle time and scrap, a cost that belongs in the quote rather than in a discount. As-cast is a different number: ISO 8062-3 DCTG grades by drawing, there is no ±0.05 mm as-cast promise, and NADCA’s product specification standards are where those grades and the machining allowances are written. The tolerance stack is set by datums and setups before it is set by the machine.
Draft is the fourth lever and the cheapest to fix on paper. One degree over 100 mm of wall buys 1.75 mm of clearance; half a degree buys 0.87 mm, and that is where torn flanks and polish marks come from.

What the change costs on the other side
Every feature change buys unit cost with tooling, validation or process window, and the bill arrives once, early, while the saving arrives every year. The trade is worth making, but it has to be priced rather than assumed.
Tooling comes first. A change before steel is cut is a drawing revision; the same change after T1 is a weld, a patch insert or a new slide, with a lead time attached. That is why the review belongs in the DFM window, before the die layout is frozen.
Validation comes second. A moved datum or a new wall section changes the control plan, the PFMEA and the inspection programme, and under PPAP it usually means a fresh submission with dimensional results, material certificates and a capability study. AIAG’s quality core tools set that discipline, and they explain why a “free” change in month nine can cost more than the saving it releases.
Process window is third, and the one that hides. A thinner wall can move casting scrap from a few percent into double digits, and five points of scrap on a machined housing eats the metal saving that justified it. At the edge of the 1.5 mm band, the quote carries a yield assumption and the PPAP run tests it.
What should not be value-engineered is the acceptance criteria. Leak rate, Cpk on functional dimensions, alloy certificates and cleanliness are the customer’s requirement, not a cost lever, and Cpk 1.67 on a safety part stays 1.67. The costs that never show on the quote usually start with an acceptance line that was quietly relaxed.
Which process the volume can pay for
Below roughly 2,000 pieces a year the tooling rarely amortizes and another process usually wins; above 10,000, HPDC with single-setup machining is hard to beat on a machined housing. Part size or a leak specification can move those bands.
| Annual volume | Process that usually wins | Where the cost sits | When the rule breaks |
|---|---|---|---|
| Under 2,000 | Sand or gravity casting from a pattern, or CNC from billet | Pattern or billet and machine time; almost no tooling | The geometry needs pressure-tight thin walls |
| 2,000–10,000 | HPDC with a simple die, or gravity where walls are thick | Tooling amortization dominates | Die cost cannot be spread; a shared tool may be the only way |
| 10,000–50,000 | HPDC, one die, single-setup machining | Metal and machining | The leak spec forces 100% test and extra stations |
| Above 50,000 | HPDC with hard tooling, automation, a second die for capacity | Metal, cycle time, yield | The part exceeds 3050T or needs more than one machining setup |
The arithmetic is tooling divided by volume. €150,000 over 8,000 parts is €18.75 per part before the first chip; the same tool over 80,000 parts is €1.88. Nothing else in the quote moves by a factor of ten with volume, so a low-volume programme should not ride a high-volume process.
Machine size belongs in the same conversation. We run 13 cells from 350T to 3050T, and projected area and shot weight pick the cell rather than the tonnage on the brochure. A part that only fits a 3050T machine carries a different amortization from one that runs on an 800T. A DFM review before the die is cut tests that arithmetic against the layout, because gate position, overflow volume, slide count and machining datums all move when a wall moves.
How to run the review without turning it into a price fight
Run it as a function review: name what each feature does, delete or loosen the ones with no function, then price what is left. A cost review argues down from the quote; a function review removes work from the drawing.
Five steps. Weigh the blank against the part. List every machined face with the function it serves (seal, locate, bear, cosmetic) and mark the ones with no mating part.
Then give each dimension a tolerance class and challenge any ±0.05 mm that touches no bearing or seal. Check draft and slide count against ejection rather than against how the model looks. Re-quote and compare annual spend, not piece price.
The method is older than die casting. Function analysis and the job plan behind it come from value engineering as formalised in transport and defence programmes, and the FHWA’s value engineering programme still runs the sequence: information, function analysis, creative, evaluation, development, recommendation. The function is named before the cost is attacked.
Timing decides the return. A review at RFQ stage changes a drawing, after T1 it changes a die, after SOP it changes a part number. We have sat in one where the only surviving recommendation was a 1.5° draft change, because the wall was already priced into a tool cut the month before.
Frequently asked questions
How much can value engineering take out of a die casting price?
On a drawing that has never been reviewed, a double-digit share of piece price is common in our experience, and it usually comes from two or three features rather than a redesign. The number has to be built from blank weight, machined face count and tolerance class, not promised as a percentage. A supplier offering 30% off the same drawing is changing the yield assumption or the tooling, and you meet that difference later.
Is it cheaper to cast closer to net shape or to machine more?
Cast closer for faces that only need to be flat or to clear something; machine the faces that seal, locate or carry a bearing. Moving a face to as-cast saves an operation and the allowance metal above it, but it also moves the tolerance from ±0.05 mm to an ISO 8062-3 DCTG grade, which is a different promise to the assembly line.
Does a thinner wall always reduce cost?
No. Metal falls roughly in proportion to thickness, but scrap, fill risk and die thermal balance rise as the wall approaches the 1.5 mm floor. Taking 0.8 mm off a 3.2 mm wall is usually a saving; taking the same 0.8 mm off a 2.2 mm wall is usually a yield experiment with the customer’s name on it.
When is it too late to change the drawing?
After the die layout is frozen, every change becomes tooling: a weld, a patch, a new slide, and a PPAP re-submission. The cheap window is the DFM review before steel is cut, and the second-cheapest is the T1 sample, when a change can still ride on the die’s first correction.
The cheapest quote is not the one with the lowest rate. It is the one whose drawing has the fewest features that exist because nobody asked what they were for.