The anodizing temperature of die-cast alumina coloring is generally below 23 °C. If the temperature is too high, the consumption of cold sealant will be large, and the surface will turn green.When di...
Do you need electricity:Anodizing is carried out under high-voltage electrical conditions and is an electrochemical reaction process. Chemical anodizing is a chemical reaction that does not require el...
The technology of conventional overall quenching has been difficult to meet the requirements on high surface wear resistance and toughness of the die casting mold.Surface strengthening treatment can n...
The chemical composition inspection, test methods, inspection standards and re-inspection of aluminum die-casting molds must meet the standards of GB/T15115. The chemical composition of the sample pro...
The chemical properties of aluminum alloys are relatively active, so aluminum alloy die casting components are prone to oxidation and corrosion under natural conditions. In order to improve the corros...